by Vetinari » Wed Nov 28, 2012 6:45 pm
ABS is fine with boiling H20 temp.s (I've used it to fix a mould defect on one of my hujoos) but I've got a feeling 270F might be a tad high wrt it going squishy - if wiki is to be trusted Tg is at 105 °C (221 °F), so it'll probably be kinda soft at that temp and might warp under it's own weight (But not sure)
Crafty people say that 240C is best for actually fiddling with the stuff and getting it to stick to things, so you'd still be 100C short of runny plastic... argh sorry not a very helpful answer! I think you'd be best sticking to the boil cure method if possible since that definitely wont do anything to the ABS, you might get away with the oven but I'd be unwilling to risk it myself